    5 factors for the blackening of die-casting parts



    • Aluminum alloy castings are the use of metal casting. Metal aluminum and aluminum alloys have good fluidity and plasticity, but they tend to turn black in the end.


    1. The process design is unreasonable. Improper handling of die castings after cleaning or pressure inspection, resulting in rapid mold growth.

    2. Warehouse management is not in place. Die-casting parts are stored at different heights, and mold conditions are unequal.

    3. The internal factors of aluminum alloy. The die-casting manufacturer did not do any cleaning after die-casting and CNC, or just rinsed with water. Mold release agent, cutting fluid, saponification fluid, and other stains remain on the surface of die-cast aluminum. These stains accelerate the blackening of the die spots on the die casting.

    4. The external environmental factors of aluminum alloy. Aluminum is easy to oxidize and become black or moldy under certain temperatures and humidity.


    5. Improper choice of the cleaning agent. The selected cleaning agent is highly corrosive, causing corrosion and oxidation of die-cast aluminum.

    aluminum-part.jpg

    Related News
    • Process Flow of Friction Welding

      Process Flow of Friction Welding

      Friction welding is one of the welding methods of hot compression welding. The welding efficiency can reach 30~70%. Generally, friction welding with a large dynamic friction coefficient has higher eff...
    • How to prevent scratches when the deburring machine is working

      How to prevent scratches when the deburring machine is working

      In the production of aluminum alloy die-cast parts, burrs are the most common problem during the metal-cutting process. To ensure the smoothness of the workpiece, workers often add a deburring process...
    • 3 commonly used modifiers for aluminum alloys

      3 commonly used modifiers for aluminum alloys

      Aluminum alloy modification is the addition of small amounts of substances to molten metal. It promotes the internal growth of molten metal. In the aluminum alloy manufacturing process, modification t...
    We use cookies to offer you a better browsing experience, analyze site traffic and personalize content. By using this site, you agree to our use of cookies. Visit our cookie policy to learn more.
    Reject Accept